| EN no. | EN designation | Cu % | Pb % | BS | UNS | IS | Typical use | AirGrip |
|---|---|---|---|---|---|---|---|---|
| CW614N | CuZn39Pb3 | 57.0–59.0 | 2.5–3.5 | CZ121Pb3 | C38500 | IS 319 Type I | Free-cutting: turned parts, glands, inserts, terminals | Standard |
| CW617N | CuZn40Pb2 | 57.0–59.0 | 1.6–2.5 | CZ122 | C37700 | — | Hot forging: fittings, valve bodies | Standard |
| CW603N | CuZn36Pb3 | 60.0–62.0 | 2.5–3.5 | CZ124 | C36000 | — | Free-cutting, higher copper | — |
| CW602N | CuZn36Pb2As | 61.0–63.0 | 1.7–2.8 | CZ132 | C35330 | — | Dezincification-resistant (DZR): drinking-water fittings | On request |
| CW511L | CuZn38As | 61.5–63.5 | ≤ 0.2 | — | — | — | Low-lead DZR: drinking water, lead-free markets | On request |
| CW724R | CuZn21Si3P | 75.0–77.0 | ≤ 0.10 | — | C69300 | — | Lead-free, high strength | On request |
| CW508L | CuZn37 | 62.0–64.0 | ≤ 0.1 | CZ108 | C27200 | — | Cold forming, stamping | — |
| CW509L | CuZn40 | 59.5–61.5 | ≤ 0.3 | CZ109 | C28000 | — | Low-lead hot forming | — |
| CW717R | CuZn38Sn1As | 59.0–62.0 | ≤ 0.2 | CZ112 | C46400 | — | Naval brass: marine parts | — |
Nearest equivalents; always check the specification your drawing calls up. Cu and Pb are composition limits from EN 12164 / 12165 / 12163. "—" in the AirGrip column = ask us. Guides: CW614N vs CW617N · lead-free and DZR brass.